PRAZI Platen met bewerkingstoegift 500 mm
Selecteer maat
52 |
---|
62 |
72 |
83 |
93 |
103 |
113 |
123 |
133 |
143 |
153 |
163 |
173 |
183 |
193 |
203 |
213 |
223 |
233 |
243 |
253 |
263 |
273 |
283 |
293 |
303 |
313 |
323 |
333 |
343 |
353 |
363 |
373 |
383 |
393 |
403 |
413 |
423 |
433 |
443 |
453 |
463 |
473 |
483 |
493 |
503 |
10.4 | 15.4 | 20.4 | 25.4 | 30.4 | 40.4 | 50.4 | 60.4 | 70.4 | 80.4 | 90.4 | 100.4 |
---|---|---|---|---|---|---|---|---|---|---|---|
|
|
|
|
|
|
|
|||||
|
|
|
|
|
|
|
|
||||
|
|
|
|
|
|
|
|
|
|||
|
|
|
|
|
|
|
|
|
|
||
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
- Aanvullende informatie
Warmwerkstaal
(X37CrMoV5-1)
Hoge taaiheid bij hoge temperaturen, zeer slijtvast, zeer goede warmte-geleiding, goede ontlaatbestendigheid en uitstekend luchthardbaar
Waterkoelbaar, nitreerbaar, goed te polijsten, erodeerbaar.
Textureren goed mogelijk
Toepassing
Drukgiet-, warmextrusie messen. Schaarmessen warm/koud. Smeed- en andere warmwerkgereedschappen
Uitvoering
In 500 mm en 1030 mm lengte met opmaat in breedte en dikte, in
plaatvorm en in vierkant.
Zacht gegloeid
Max. 229 HB (max. 770 N/mm²)
Richtanalyse
C | Si | Cr | Mo | V | |
0,37 | 1,0 | 5,3 | 1,3 | 0,4 | in % |
Warmtebehandeling
Spanningsarm gloeien: 650 – 680 °C
Zacht gloeien: 750 – 780 °C
Harden: 1000 -1030 °C
Afschrikken: Olie, lucht of warm bad
Ontlaten: 530 – 680 °C
Speciale warmtebehandeling:
Bij eroderen of nitreren moet de ontlaattemperatuur boven de secundair maximum hardheid liggen. Twee keer ontlaten is aan te bevelen